Influence of Welding Parameters and Tool Pin Profile on the Microstructure and Mechanical Properties of Dissimilar Friction Stir Welded AA2024-T3 to AA6061-T6 Alloys
This study aims to produce joints from dissimilar Al alloys welded by the FSW process with a minimal defect rate. The investigation focuses on the mechanical behavior and microstructural characteristics of 2 mm-thick dissimilar Al alloys, AA2024-T3 + AA6061-T6. The parameters of the welding process were welding speed,...