The microstructure and tensile properties of TIG-welded 316H joints after aging at 600 °C for up to 2000 hours were investigated. In base metal (BM), M23C6 carbides precipitated along grain boundaries after 500 hours and coarsened, while in weld metal (WM), δ-ferrite decomposed into M23C6 within 100 hours. The faster a...
Xiang-Bin Ding, Yi-Qiang Yao, Yong-Zhi Dong et al.· Journal of Physics, Conferen...· 0 citations