Physics-guided inverse design of Co-based superalloys using machine learning and multi-objective optimization for enhanced $\gamma'$ solvus temperature

Sep 2026 · 0 citations · 47 references
Physics

Abstract

The discovery of next-generation Co-based superalloys with improved high-temperature stability is hindered by the vast compositional design space and complex interactions among alloying elements governing gamma-prime phase stability. This study presents a physics-informed machine learning framework for the inverse design of Co-based superalloys with higher gamma-prime solvus temperature while accounting for alloy density. Four descriptors representing atomic size mismatch (delta-MV), mixing enthalpy (Delta-Hm), electronegativity mismatch (delta-EN), and valence electron concentration mismatch (delta-VEC) were used to characterize the chemistry governing phase stability. Regression algorithms were evaluated using leave-one-out cross-validation, with Gaussian Process Regression (GPR) achieving the best performance (R2 = 0.932, RMSE = 34.7 deg C, and MAE = 25.9 deg C). The probabilistic nature of GPR enabled uncertainty-aware Bayesian optimization for exploring the uncharted composition space. Non-dominated Sorting Genetic Algorithm II (NSGA-II) and Genetic Algorithms were used to simultaneously increase gamma-prime solvus temperature and reduce alloy density. The optimization generated numerous previously unexplored Co-based alloy compositions, with predicted gamma-prime solvus temperatures of 1248-1353 deg C, including candidates approaching or exceeding the maximum value in the experimental dataset. Descriptor analysis identified atomic size mismatch and mixing enthalpy as key factors governing gamma-prime stability, while principal component analysis confirmed that the proposed alloys occupy chemically relevant descriptor regions. This physics-informed inverse design framework provides an efficient route for identifying high-performance Co-based superalloys and can be adapted to other advanced structural alloys.

View source

We use cookies to run the site and, with your consent, for analytics and to show ads. See our Cookie Policy.