Abstract

This study evaluated the influence of the manufacturing method and cementation protocol on the fracture load of zirconia molar crowns. A total of 32 full-contour crowns with a wall thickness of 1 mm were fabricated from 3 mol% yttria-stabilized tetragonal zirconia polycrystal (3Y-TZP). Sixteen crowns were produced by 3D printing (LithaCon 3Y 210, Lithoz) and 16 by milling (e.max ZirCAD LT, Ivoclar Vivadent). Within each manufacturing group, eight crowns were adhesively luted with a dual-cure resin cement (Bifix QM, VOCO) and eight were conventionally cemented with a glass ionomer cement (Ketac Cem, Solventum). All crown–die complexes underwent thermomechanical aging (6000 thermal cycles between 5 °C/55 °C; 1.2 × 106 cycles at 50 N) as a correlate of five years of clinical service, followed by axial loading to failure. The statistical analysis was a two-way ANOVA on log10-transformed fracture loads with manufacturing and cement as fixed effects (α = 0.05). All crowns survived thermomechanical loading without failure. Milled zirconia crowns showed significantly higher fracture loads when adhesively luted (7162 ± 1294 N) compared with conventional cementation (4021 ± 1126 N; p < 0.001). In contrast, no significant differences were observed between adhesive (4986 ± 1301 N) and conventional cementation (5581 ± 1618 N) for 3D-printed zirconia crowns. Additively manufactured crowns exhibited greater variability in fracture loads (broader interquartile ranges) than their milled counterparts. Two-way ANOVA detected a significant Manufacturing × Cement interaction (p < 0.001), indicating that the effect of cementation differed by manufacturing route. Adhesive cementation increased fracture load for milled zirconia, whereas no statistically significant cementation effect was detected for 3D-printed zirconia under the present conditions. Given the sample size and the observed variability, the study was powered to detect very large effects but not medium or small ones; therefore, this non-significant difference should not be interpreted as proof of no effect.

Read PDF

We use cookies to run the site and, with your consent, for analytics and to show ads. See our Cookie Policy.