Skip to content
Open access

Effect of deposition variables on solidification behavior and mechanical response of LMD-fabricated Ti-6Al-4V alloy clads

2026 · Matéria · 0 citations · 43 references

Abstract

ABSTRACT Laser Metal Deposition (LMD) offers a versatile pathway for near-net-shape fabrication of high-performance titanium components. In this work, Ti-6Al-4V thin-wall structures were fabricated using orthogonally designed experiments to study coupled effects of laser output intensity (800–1400 W), scanning rate (4–12 mm/s) and feedstock mass flow (6–14 g/min). Optimal deposition window was identified at 1100 W, 10 mm/s, 8 g/min, producing geometrically stable tracks with minimum dilution, free of pores. Microstructural characterization revealed epitaxial β-columnar growth at fusion boundary transitioning to refined α + β colonies, with localized martensitic α′ observed at higher cooling rates. Estimated thermal gradients and solidification velocities enabled interpretation through a solidification-mode transformation framework, linking thermal history to grain morphology. The as-deposited clad hardness ranged from 385–455 VHN, gradually decreasing toward mid-height due to tempering from successive reheating, while heat-affected zone exhibited 355–380 VHN and the substrate retained ~340 VHN. Such gradients correlated with microstructural refinement and localized cooling conditions. Anisotropic tensile behavior, attributed to directional solidification and interlayer reheating, confirmed a microstructure–property relationship consistent with LMD-induced thermal cycling. Overall, the study highlights that scanning rate exerts dominant control over melt-pool geometry, grain refinement, and mechanical response, while inappropriate energy density promotes excessive coarsening.

Read PDF

We use cookies to run the site and, with your consent, for analytics and to show ads. See our Cookie Policy.