Influence of welding current on the bending failure mechanism of Ni625 alloy overlay on 4130 steel via the GTAW-P process
Abstract
4130 Cr-Mo low-alloy high-strength steel is widely used in oil and gas wellhead equipment, but surface failure becomes prominent under corrosive and erosive service environments. In this paper, Ni625 alloy overlays were deposited on 4130 steel by pulsed gas tungsten arc welding (GTAW-P) at welding currents of 200 A, 215 A, and 230 A. The macro-forming quality, 180° bending behavior, low-temperature impact toughness, hardness, fracture morphology, and fracture microzone element distribution were systematically analyzed. The results show that increasing welding current raises heat input from 0.56 kJ/mm to 0.64 kJ/mm and deteriorates bending failure from weld-edge cracking to through brittle fracture along the fusion line/HAZ, whereas impact toughness and hardness remain qualified. SEM-EDS results show that the bending failure mechanism is the coupled action of oxide-inclusion bands and Ni/Cr depletion at the fusion line. The black-line fracture zone contains 7.35%-19.25% oxygen and a minimum Ni content of 27.70%, which weakens the interfacial metallurgical bond. Therefore, reducing heat input is essential for improving ASME IX bending compliance.