Molecular Bridging of Ceramic–Polymer Interfaces Enables Fast Ion Transport and Long‐Life Solid‐State Lithium Metal Batteries

Sep 2026 · Advanced Functional Materials · Vol 36 · 0 citations · 43 references

Abstract

Composite solid electrolytes (CSEs) are promising for high‐energy solid‐state lithium metal batteries, yet weakly coupled ceramic/polymer interfaces often induce filler aggregation, interfacial defects, and discontinuous Li+ transport. Here, we establish a molecular‐bridging strategy using bifunctional PFDTES to couple LLZTO with a fluorinated polymer framework. PFDTES chemically anchors to hydroxylated LLZTO through hydrolysis–condensation reactions, while its perfluorinated segment enhances affinity toward PVDF‐HFP, thereby transforming weakly contacted ceramic/polymer interfaces into more strongly coupled interphases. This dual‐ended molecular bridging suppresses filler aggregation and interfacial defects while reshaping the local Li+ coordination environment. The resulting polar interfacial environment weakens Li+–TFSI− association and strong local Li+–ether oxygen coordination, thereby lowering the kinetic barrier for Li+ migration across heterogeneous phases. Consequently, PLF‐CSE achieves an ionic conductivity of 5.05 × 10−4 S cm−1 at 30°C, a Li+ transference number of 0.72, and an electrochemical stability window of 5.12 V. More homogeneous Li+ flux, together with a LiF/Li3N‐rich interphase, enables stable lithium plating/stripping for over 6000 h, while LFP|PLF‐CSE|Li cells retain 92.9% of their capacity after 1000 cycles at 2 C. This work highlights the critical role of molecular bridging in regulating Li+ transport across ceramic/polymer interfaces, offering a rational strategy for designing high‐performance CSEs.

View source

We use cookies to run the site and, with your consent, for analytics and to show ads. See our Cookie Policy.