Ambient-atmosphere ultrasonic atomization of low-melting-point wood’s alloy powders: process optimization, atomization mechanism, and solderability
Abstract
Low-melting-point alloy powders are crucial for temperature-sensitive electronic packaging. However, preparing quaternary Wood’s alloy powders containing volatile elements (Pb, Cd) via traditional atomization often causes compositional deviation and oxidation. Herein, 13.3Sn–50Bi–26.7Pb–10Cd (wt%) Wood’s alloy powders were prepared using ambient-atmosphere ultrasonic atomization. The effects of ultrasonic amplitude, heating tank temperature, and vibration stage temperature on powder characteristics were systematically investigated. Furthermore, the atomization mechanism was studied using high-speed photography, and the solderability of the optimized powder on 304 stainless steel was evaluated. Results indicate that increasing ultrasonic amplitude from 20 to 30% regulates powder quality, decreasing the median diameter (D50) from 77.78 to 71.07 μm, narrowing the size span from 2.29 to 1.96, and improving sphericity. An optimal heating tank temperature of 90–150 °C maintained low oxygen content (77–79 ppm) and good powder morphology, while temperatures above 150 °C increased oxygen content to 110 ppm and deteriorated sphericity. A room temperature vibration stage yielded the highest sphericity. Phase analysis confirmed the presence of β–Sn, Bi, Pb, Cd, and Pb7Bi3 intermetallics, with Pb7Bi3 acting as a solute sink for Bi to lower the melting temperature. High-speed imaging revealed that atomization is driven by the synergistic effect of Faraday capillary waves and acoustic cavitation, triggered by a critical liquid film thickness. Finally, joints soldered with the optimized powder exhibited an average shear strength of 25 ± 5.0 MPa, demonstrating excellent suitability for near-room temperature electronic interconnections.