PLA/BioAlSr composite films for tendon–bone interface regeneration: effect of bioactive glass content on morphology, mechanical behavior, degradation and bioactivity
Abstract
One of the major challenges in implant materials engineering is combining mechanical strength, moldability, biocompatibility, bioresorbability, and osteoactivity within a single material. This work develops poly(lactic acid) (PLA) films loaded with a strontium- and alumina-containing bioactive glass (BioAlSr), explored as a candidate material for metallic-implant coatings and, prospectively, tendon–bone interface grafts. Melt-quenched glass powder (mean diameter 5 µm) was incorporated at 15, 30, 50 and 70 wt% by solvent casting. Characterization covered microscopy with TGA, EDS, XRD, tensile testing, swelling in phosphate-buffered saline (PBS) with pH monitoring, cytotoxicity and bioactivity in simulated body fluid (SBF). Particles were mechanically embedded, with no evidence of strong interfacial bonding. Tensile strength peaked at 15 wt% (15 ± 1 MPa) and fell sharply already by 30 wt% (6.1 ± 1.3 MPa), continuing to decline at 50–70 wt% (3 ± 2 to 2.5 ± 6 MPa); elongation at break fell from 61 ± 17 % for neat PLA to 13 % at 15–30 wt% and below 5 % at 50–70 wt%, while Young's modulus (63–72 MPa) was comparatively insensitive to glass content. After 28 days in PBS, swelling ranged from 2.1 % (30 wt%) to 8.6 % (70 wt%) against 2.7 % for neat PLA, and pH rose from 7.2 to 9.0–10.6 for loadings ? 30 wt%, remaining near 7.3 for neat PLA and 15 wt%. In neutral red uptake, undiluted extract gave 89 % viability for 15 wt% and 66 % for 30 wt%, against 46 % for neat PLA (NCTC clone 929); the 50 and 70 wt% films reduced viability to 63 % at 100 mg mL?¹ (NIH/3T3). No composite reached IC50, and all were less cytotoxic than neat PLA. After SBF immersion, all glass-loaded films developed a crystalline calcium-phosphate phase while EDS confirmed progressive Ca and P surface enrichment, supporting apatite-like mineralization. Glass content therefore trades mechanical performance against degradation and bioactivity; 15–30 wt% was retained as the working range for its favorable combination of tensile strength and particle-dispersion homogeneity relative to 50–70 wt%, notwithstanding PVBio30's cytotoxicity falling marginally below the ISO 10993-5 threshold.