Recycling with Bitumen Emulsion of Waste Materials for Road Construction: An Experimental Analysis
Abstract
The valorisation and reuse of waste materials represent an effective strategy for improving the environmental sustainability of road construction, particularly when cold recycling techniques are adopted. Compared with conventional hot - mix processes, these technologies significantly reduce energy consumption and atmospheric emissions. Among the available approaches, the stabilization of aggregates with bitumen emulsion is widely employed, especially in the case of reclaimed asphalt pavement (RAP). Nevertheless, other industrial byproducts waste materials can also be successfully reused within a Cold Central Plant Recycling (CCPR) framework. This study presents the results of a laboratory investigation on bitumen emulsion bound mixtures designed for pavement base courses and characterized by an aggregate skeleton entirely composed of waste materials, namely reclaimed asphalt pavement (RAP), steel slag, coal ash and glass waste, combined in different proportions. The experimental program was structured in two main phases. First, a preliminary characterization of each waste material was performed, focusing on both physical properties and environmental compatibility, including toxicological aspects, in order to verify their suitability for reuse in road engineering applications. In the second phase, a comprehensive mechanical characterization of the bitumen emulsion stabilized mixtures was conducted. The experimental testing program included indirect tensile strength (ITS) tests, indirect tensile stiffness modulus measurements performed at three temperatures (10°C, 25°C and 40°C), and repeated load axial tests carried out at 30°C to evaluate the mixtures’ resistance to permanent deformation. In addition, indirect tensile strength tests were performed on water - conditioned specimens to assess the moisture susceptibility of the mixtures. The results demonstrated satisfactory mechanical performance for several mixture compositions. Indirect tensile strength values at 25°C on dry specimens reached up to 0.44 MPa, while stiffness modulus values at the same temperature ranged up to approximately 3,000 – 4,500 MPa, depending on the mixture composition and testing conditions. The mixtures also exhibited adequate resistance to moisture damage, confirming the effectiveness of bitumen emulsion in providing cohesion and durability even when unconventional aggregates are used. The measured mechanical properties were compared with the requirements specified in the main Italian technical specifications for bitumen emulsion bound mixtures used in pavement base layers. The comparison confirmed that the investigated materials meet the relevant acceptance criteria. Overall, the findings indicate that RAP, steel slag, coal ash and glass waste can be effectively used as complete substitutes for natural aggregates in bitumen emulsion stabilized mixtures for pavement base courses, contributing to resource conservation and supporting circular economy strategies in road infrastructure engineering.