Evaluation of the Electrochemical Behavior of the Hot-Rolled Ti–12Mo–30Nb Alloy Applied in Biomedical Implants
Abstract
β-Ti alloys are essential for biomedical applications due to their low elastic modulus, high strength, fatigue resistance, ductility, and corrosion resistance. β-metastable alloys such as Ti-12Mo-30Nb offer safer alternatives to Ti-6Al-4V by eliminating biotoxic elements (Al and V) linked to cell death and neurodegeneration. This study analyzed the microstructural, mechanical, and electrochemical properties of hot-rolled Ti-12Mo-30Nb (90% reduction). Characterization was conducted by XRD, OM, and SEM, while Vickers microhardness and impulse excitation tests were used to assess mechanical performance. The alloy exhibited a single-phase β microstructure, an elastic modulus of 72 Gpa, mitigating the “stress shielding” effect, and a hardness of 228 HV. The hardness-to-modulus ratio (H/E = 3.2) was higher than that of Ti-6Al-4V (2.9) and cp-Ti (2.6), confirming superior mechanical behavior. Electrochemical tests in Ringer’s solution revealed the formation of a stable TiO2 passive layer, with corrosion and passivation current densities of approximately 10−1 μA.cm-2 and 10 μA.cm-2, respectively. These results indicate excellent corrosion resistance and biocompatibility, demonstrating that Ti-12Mo-30Nb is a promising and safe material for medical devices compared to conventional Ti alloys.