Effectiveness of self-etching ceramic primer on the bond strength of lithium disilicate glass-ceramics: A systematic review and meta-analysis of in vitro studies.
Abstract
Purpose
This systematic review and meta-analysis compared Monobond Etch & Prime (MEP) and hydrofluoric acid followed by silane (HF + S) on the tensile and shear bond strengths (TBS/μTBS and SBS/μSBS, respectively) of lithium disilicate glass-ceramics. STUDY SELECTION This review was registered in the Open Science Framework and conducted according to the Preferred Reporting Items for Systematic Reviews and Meta-Analyses 2020 statement. PubMed/MEDLINE, Scopus, Embase, and Web of Science were searched through July 2026, complemented by manual and gray literature searches. In vitro studies comparing MEP with HF + S were included. Risk of bias was assessed using Risk of Bias for Dental Materials guide. Subgroup meta-analyses considered bond strength test, aging condition, HF concentration, and application time.
Results
Of 1,861 records, 46 studies were included. Before aging, most subgroup analyses showed comparable bond strengths between MEP and HF + S, including TBS with 4.5-5% HF for 20s and 9-10% HF for 60s. After aging, comparable TBS and μTBS were observed after 5,000 (4.5-5% HF, 20s) and 10,000 thermal cycles (9-10% HF, 20s), respectively. HF + S showed higher μTBS before aging (9-10% HF, 20s) and μSBS after aging (4.5-5% HF, 20s). Thermocycling generally reduced bond strength. All studies lacked operator blinding and adequately reported specimen randomization.
Conclusions
MEP achieved bond strengths comparable to HF + S under several laboratory conditions, although specific subgroups favored HF + S. Given methodological heterogeneity, these findings warrant cautious interpretation and do not demonstrate equivalent long-term clinical performance.