Valorization of titanium production waste for selective Fe–Ti separation and concentrate production from titanomagnetite: response-surface optimization of chloride-assisted reduction roasting

Sep 2026 · Acta Metallurgica Slovaca · Vol 32, pp. 228-240 · 0 citations

Abstract

Titanium production wastes represent an underutilized secondary resource with potential value as functional additives in metallurgical processing. This study investigates the chloride-assisted reduction roasting of high-titanium titanomagnetite concentrate using semi-coke, spent titanium chlorinator melt (SMTC), a chloride-rich titanium production waste, and CaF2 to achieve selective Fe–Ti separation. A four-factor Box–Behnken response-surface design was applied to quantify the effects of roasting temperature and semi-coke, SMTC, and CaF2 dosages on Fe grade, Fe recovery, TiO2 grade, TiO2 recovery, and iron metallization. RSM identified roasting temperature as the dominant process variable and delineated a broad high-performance region. The practically optimal conditions were 1200 °C, 20 wt.% semi-coke, 30 wt.% SMTC, and 4 wt.% CaF2, yielding a magnetic fraction containing 91.24 wt.% Fe at 91.94% recovery and a non-magnetic fraction containing 62.78 wt.% TiO2 at 96.04% recovery. Compared with NaCl, SMTC provided a substantially better balance between iron metallization and titanium partitioning. XRD and EPMA revealed extensive formation and coalescence of metallic α-Fe together with enrichment of rutile and magnesium titanate in the non-magnetic product. These findings demonstrate that chloride-rich titanium production waste can serve as an effective process additive for selective Fe–Ti separation, providing a dual pathway for titanomagnetite beneficiation and metallurgical waste valorization. 

Read PDF

We use cookies to run the site and, with your consent, for analytics and to show ads. See our Cookie Policy.