Skip to content
Open access

Improved wideband electromagnetic performance in La3+ substituted Mn–Zn spinel ferrites: structure–microstructure regulation of grain-boundary non-Debye relaxation

Nov 2026 · RSC Advances · 0 citations · 69 references
Medicine

Abstract

Grain-boundary related electrical relaxation and microstructural evolution are important factors in the frequency-dependent response of Mn–Zn ferrite. Here, La3+ substituted Mn–Zn ferrites, were synthesized by a solid-state route (calcination at 800 °C for 4 h and sintering at 1200 °C for 6 h). Rietveld refinement confirms a spinel-dominant cubic phase for all compositions. A minor orthorhombic phase appears above a La3+ threshold and remains below about 4%. The lattice parameter shows only small variation (about 8.41–8.45 Å). SEM and density analysis show grain refinement from about 1.87 µm to 1.07 µm and a non-monotonic porosity evolution (about 16–36%). Room-temperature hysteresis loops confirm soft magnetic behavior. The saturation magnetization increases strongly and reaches 33.96 emu g−1 at an intermediate La3+ level. Wideband measurements show composition-dependent relatively stable real permeability and strongly reduced magnetic loss at high frequency. Dielectric and impedance spectra show strong low-frequency dispersion consistent with Maxwell–Wagner interfacial polarization. Electric modulus and Cole–Cole plots exhibit depressed arcs, indicating non-Debye relaxation with distributed relaxation times dominated by grain boundaries. Nyquist fitting separates grain and grain-boundary responses and shows composition-tunable interfacial barrier behavior. Overall, the results demonstrate that La3+ substitution modifies the structural and microstructural state of Mn–Zn ferrites, establishing a composition-dependent balance between magnetic properties, interfacial relaxation, and high-frequency electromagnetic response.

Read PDF

We use cookies to run the site and, with your consent, for analytics and to show ads. See our Cookie Policy.