Effect of Al3Fe particle addition on the structure and mechanical properties of Al – 20 vol. % Sn alloy fabricated by selective laser melting

2026 · Physics and Chemistry of Materials Treatment · 0 citations

Abstract

This paper examines the structural features and related mechanical properties of the Al – 20 vol. % Sn – 10 vol. % Al3Fe alloy produced by selective laser melting (SLM). The scanning speed during SLM was kept constant at 1.2 m/s, while the laser power (P) was varied from 50 to 170 W in 40 W increments. To produce a composite of the given composition, a mixture of commercial powders of ASD-1 grade aluminum, PO-1 tin, and Al3Fe powder prepared by grinding a sintered briquette of stoichiometric composition in a ball mill was used. The influence of P during SLM on the evolution of the alloy structure was assessed using electron microscopy and X-ray diffraction data. The structure of the material was examined using thin sections oriented along the building direction of the specimens during SLM. The relationship between the structure and the mechanical properties of the alloy was determined by analyzing the plastic flow curves σ(ε) of compressed specimens cut from the middle of alloy samples produced by SLM. It was found that the studied alloy with a relatively uniform distribution of components throughout the sample volume, in which there are virtually no cracks, can be produced only at a high volume density of radiant energy, achieved at P = 170 W, which ensures a high melt temperature and its high mobility. Moreover, the iron aluminides present in the alloyed powder mixture act as an inert additive that prevents active convective mixing of low-melting components. As a result, the produced Al – 20 vol. % Sn – 10 vol. % Al3Fe alloy had a finely dispersed structure with an aluminum matrix grain size of less than 1 µm. Its strength (ultimate strength σU = 146 MPa) was much higher compared to the base Al – 20 vol. % Sn alloy (σU = 90 MPa), containing an equivalent amount of soft tin phase, but its ductility was low, less than 1 %.

View source

We use cookies to run the site and, with your consent, for analytics and to show ads. See our Cookie Policy.