Skip to content
Open access

Experimental Investigation of Post-Fire Mechanical Behaviour of Structural Steel S235JR Subjected to Fire Loading and Different Cooling Methods

Nov 2026 · Inżynieria Mineralna · 0 citations · 9 references

Abstract

Fire is one of the most severe accidental actions affecting building structures, and steel elements exposed to high temperatu res may retain load - bearing capacity even after the fire has been extinguished. Since visual inspection alone is insufficient to assess the safety of fire - damaged steel elements, reliable knowledge of their post - fire mechanical behaviour, including both the mechanical properties and the shape of the stress - strain response, is essential for structural diagnosis. The aim of this study was to experimentally investigate the post - fire mechanical behaviour of structural steel S235JR after fire loading, and to evaluate how the maximum temperature reached and the subsequent cooling method affect the resulting stress - strain diagrams as well as the residual yield strength, tensile strength, modulus of elasticity, and ductility of the material. A total of 45 standard tensile test specimens made of S235JR steel (five per group) were heated to nominal temperatures of 500 °C, 600 °C, 700 °C, and 800 °C, with the heating regime approximating the ISO 834 fire curve. For specimens heated to 800 °C, an additional 30 - minute holding period was applied to allow the austenitizing transformation, which begins at approximately 723 °C, to approach completion before cooling. One series at each temperature was cooled rapidly by water quenching, and a second series slowly in an isothermal chamber. A reference series was tested at 20 °C without thermal loading. Residual yield strength (R e ), tensile strength (R m ) and elongation (A) were determined from the stress - strain diagrams and compared between groups using Welch's t - test, one - way ANOVA, and linear regression against temperature. Reference specimens showed R e = 282.9 MPa, R m = 420.8 MPa and A = 36.6%. Up to 700 °C, R e and A remained close to reference values for both cooling methods (R e 283 – 296 MPa, A 35 – 37%), with no significant effect of cooling method (p > 0.05), while R m was already significantly higher after water quenching than after slow cooling (p < 0.05). At 800 °C, all properties diverged significantly between the two methods (p < 0.05): slow cooling reduced R e to 253.9 MPa (90% of reference) and increased A to 41.6% (113%), fully meeting EN 10025 - 2 requirements, whereas water quenching raised R m to 514.5 MPa, exceeding the standard range for S235JR, while A collapsed to 17.9% (49% of reference), below the required minimum of 26%. In all five water - quenched 800 °C specimens the distinct yield plateau disappeared, with yield strength evaluated as offset R p0.2 instead of R eH. Up to 700 °C, residual yield strength and ductility of S235JR are governed mainly by temperature, largely independent of cooling method, while tensile strength is already measurably cooling - sensitive. Above the eutectoid temperature of about 723 °C, cooling method becomes decisive: slow cooling preserves a ductile, standard - compliant material, whereas rapid water quenching produces a stronger but markedly less ductile material with a suppressed yield plateau, failing the minimum elongation requirement. Both the maximum temperature reached and the post - fire cooling method must therefore be considered when assessing the residual load - bearing capacity of fire - affected S235JR steel elements.

Read PDF

We use cookies to run the site and, with your consent, for analytics and to show ads. See our Cookie Policy.