Prior‐Guided SEM Image Segmentation Enables Quantitative Morphology Assessment and Process Optimization in Perovskite Solar Cells

Sep 2026 · Advances in Materials · Vol 38 · 0 citations · 52 references
Medicine

Abstract

Perovskite film morphology strongly affects charge transport, nonradiative recombination, and power conversion efficiency, yet scanning electron microscopy (SEM) remains largely qualitative. Here, a prior‐guided SEM analysis framework converts routine micrographs into class‐resolved masks, quantitative morphology descriptors, and a compact SEM‐Derived Morphology Quality Index (MQI). YOLO‐derived grain‐center priors guide U‐MambaBot segmentation, while Class‐Probability TV Regularization improves local coherence. Six descriptors are extracted from the segmented ABX3${\rm ABX}_3$ matrix and PbI2${\rm PbI}_2$ ‐like regions, from which four are selected for MQI construction. Across nested, publication‐grouped, and within‐publication validation schemes, MQI retains a significant monotonic association with power conversion efficiency (Spearman ρ=0.34$\rho = 0.34$ and 0.42). In annealing‐time and additive‐concentration studies, MQI reproduces film‐ and device‐level performance trends and identifies the same optimal processing conditions. Without refitting, it further tracks reported morphology–performance trends across 12 independent studies and 37 processing conditions, yielding a pooled within‐study Spearman ρ=0.90$\rho = 0.90$ (publication‐level bootstrap 95% CI 0.79–1.00). This framework enables quantitative, morphology‐aware SEM screening and process‐condition ranking for perovskite films.

Read PDF

Similar papers

Oct 2026

LI-SEMIS: High-precision instance segmentation for SEM images of lithium-ion batteries ternary materials.

Accurate instance segmentation of electrode microstructures is essential for establishing processing-structure- property linkages and enabling automated quality assurance in lithium-ion batteries (LIBs) manufacturing. However, dense packing, strong adhesion, and multiscale morphology in LIBs ternary materials scanning...

Yu Qi, Ying-Ying Sun, Xiao-Qiang Li et al. · 0 citations
Open access Nov 2026

Image‐Derived Structure–Morphology–Activity Relationships in Cu–Zn Mixed Metal Oxide/Poly(Glycidyl Methacrylate) Nanocomposites

Cu–Zn mixed metal oxide/poly(glycidyl methacrylate) (PGMA) nanocomposites were synthesized by alkaline precipitation followed by copper‐mediated controlled radical polymerization and evaluated against Escherichia coli , Staphylococcus aureus , and Bacillus subtilis . Fourier transform infrared spe...

Haridharan Neelamegan, V. S. Remella, N. Malarvizhi · 0 citations
Open access Oct 2026

Micrometre-Scale Surface Partitioning and Morphological Anisotropy in Reacted Bioactive Glass Quantified by SEM–EDS

Reacted bioactive-glass surfaces often contain Ca–P-rich deposits beside Si-rich regions, but qualitative overlap in SEM–EDS maps cannot establish whether Ca and P are spatially associated or merely co-occur because clustered maps occupy finite areas. Here, one archived EDS field and one separate SEM field from each of...

H. Vasconcelos, M. Meirelles · 0 citations
Review Nov 2026

Deep learning-assisted TEM image analysis for morphological characterization of molybdenum disulfide catalysts.

The morphology of molybdenum disulfide (MoS2) plays a key role in its catalytic performance, as active sites are associated with the edges of its layered structure. Transmission electron microscopy (TEM) is widely used to characterize MoS2 catalysts, but manual image analysis is time-consuming and operator-dependent. H...

M. Y. Boiko, L. G. Mamyan, M. Knyazeva et al. · 0 citations
Review Open access Oct 2026

Post‐Processing Strategies for Laser‐Scribed Grooves in Perovskite Solar Modules: Mechanisms, Trade‐Offs, and Engineering Guidelines

Monolithic integration is widely regarded as a practical pathway toward scalable perovskite solar modules (PSMs). Despite substantial progress in understanding and mitigating laser‐scribing‐induced damage, laser‐scribed groove regions remain important localized sources of performance loss and degradation that can affec...

Cheng Peng, Zhi-Peng Li, Da-Chang Liu et al. · 0 citations

We use cookies to run the site and, with your consent, for analytics and to show ads. See our Cookie Policy.