Sep 2026· Journal of the American Chemical Society· Vol 148 40, pp.
43673-43681
· 0 citations· 35 references
Medicine
Abstract
Aqueous zinc batteries (AZBs) are promising for large-scale and safe energy storage, yet their practical application is hindered by dendrite growth, corrosion, and parasitic side reactions on Zn anodes. Herein, a high-modulus, charge-rich interfacial layer is constructed through electrostatic coupling of poly(2-acrylamido-2-methyl-1-propanesulfonic acid) (PAMPS) with polyaminopropyl biguanide (PB) to stabilize Zn anodes. The coupled interfacial layer synergistically integrates anion-cation regulation with enhanced mechanical robustness, accelerating Zn2+ desolvation, regulating ion flux, and suppressing side reactions. Meanwhile, the high-modulus yet tough interfacial layer effectively mitigates dendrite growth and buffers volume fluctuations during repeated Zn plating/stripping. As a result, the symmetric cells deliver an ultralong lifespan of over 2200 h at 1.0 mA cm-2 and 1.0 mAh cm-2, and maintain stable operation for over 800 h at 20.0 mA cm-2 with 10.0 mAh cm-2. Zn||Cu cells achieve highly reversible plating/stripping over 2000 cycles, and the Zn||NaV3O8 full cells demonstrate excellent rate capability and long-term cycling over 3500 cycles. This work provides a promising strategy for enhancing the anode stability of high-performance aqueous zinc batteries.
Artificial interfacial layers on Zn anodes are a promising route for stabilizing alkaline Zn-Ni batteries, but their practical effectiveness is often limited by a trade-off between suppressing water-induced parasitic reactions and maintaining rapid Zn-containing species transport. Herein, a hydrophobic-hydrophilic grad...
Meng-Yue Liu, Hao Tian, Gui-Sheng Guo et al.· ACS Applied Materials and In...· 0 citations
The development of aqueous zinc batteries is critically constrained by the electrode-electrolyte interfacial instability at the Zn anode. Herein, a zwitterionic dynamic buffering interface (ZDBI) is constructed by using trace glufosinate ammonium (GA). The dissociated GA- anchors onto the Zn(101) surface via its phosph...
Aqueous zinc-ion batteries offer advantages of low cost and environmental friendliness, yet their practical applications are hindered by uncontrolled dendrite growth and parasitic reactions. Herein, we introduce a gelatin electrolyte additive to stabilize the Zn/electrolyte interface and extend battery lifespan. Unli...
Si-Qi Bao, Shi-Ying Wang, Rui-Ting Yang et al.· Journal of the Electrochemic...· 0 citations
Aqueous zinc-ion hybrid capacitors (AZICs) offer the advantages of safety, low cost, and environmental friendliness, but the poor interfacial stability of the Zn anode remains a bottleneck for their large-scale energy storage applications. Certain electrolyte additives can only provide one-dimensional regulation, whi...
The development of aqueous zinc-ion batteries (AZIBs) is often limited by uncontrolled dendrite growth and detrimental side reactions occurring at the Zn anode. Herein, a multifunctional protective coating, constructed by incorporating vermiculite nanosheets (VN) into a carboxymethyl cellulose (CMC) matrix, was develop...
Xue-Hua Zhou, Jia Wang, Yan Zhang et al.· ACS Applied Materials and In...· 0 citations